Prometheus® Silver 999 Syringe, 10 g for firing from 570°C on.
There are three nozzle (English: tip) included in the Syringe. More matching Nozzles for metal clay - syringes can be found in the chapter tools modeling!
Prometheus® Silver Clay 999 gives you the opportunity to design stronger and more flexible jewelry. It does not require activated carbon or multi-step firing.
Place your dried jewelry at room temperature on a mineral fiber mat and heat the kiln at full speed to 570°C with 1 hour hold, the shrinkage is 12%.
If you would like to bend your fired pieces into bracelets or ring loops, then fire your pieces from room temperature to 700°C at full speed with 1 hour hold time, the shrinkage here is 13%.
You can still take your fired pieces out hot.
|