Prometheus® Silver Clay 999 gives you the opportunity to design stronger and more flexible jewelry. It does not require activated carbon or multi-step firing.
Place your dried jewelry at room temperature on a mineral fiber mat and heat the kiln at full speed to 570 ° C with 1 hour hold, the shrinkage is 12%.
If you would like to bend your fired pieces into bracelets or ring loops, then fire your pieces from room temperature to 700 ° C at full speed with 1 hour hold time, the shrinkage here is 13%.